Quality control in Dongguan: AQL sampling and lab reports

At Lucky Factory we check incoming parts and finished pieces by sampling, at AQL 2.5 for major and AQL 4.0 for minor defects. Our charm and pendant samples passed third-party lab tests by CTT for nickel, lead and cadmium, and a gold-plated bangle sample passed the REACH nickel release test after simulated wear.

A staff member checking a fine chain between her hands beside a green tray of finished pieces at an inspection table
Major defects
AQL 2.5
Minor defects
AQL 4.0
Defect rate
Under 1%

Control points

What is checked, how, and how often?

Control points
StageWhat is checkedMethodHow often
Before productionThe approved sample—Every order
Incoming and finished pieces (IQC, FQC)Major and minor defectsIncoming (IQC) and outgoing (FQC) inspection to GB/T 2828.1, against the AQL limits aboveEach batch, by sampling
Plating thickness0.03–3 µm, depending on the plating methodCoating thickness measurement, for PVD and electroplating in 14K and 18K gold—
Lab testsNickel release, lead and cadmium (REACH, CPSIA, CSPA), RoHS, EN 71 and ASTM F2923-20, on charm and pendant samples and one gold-plated bangleThird-party lab tests by CTTPer report (see its date)
Finish testsSalt-spray, artificial-sweat and wear tests on plated finishesOur own tests, separate from the third-party lab reports. See the salt-spray testAsk us when you order

Defects and spares

What happens to a defective piece

We mark and isolate defective pieces, rework and re-inspect the ones that can be repaired, and scrap the rest. If a sampling check fails, we inspect the whole batch before it ships. To cover the odd faulty piece, 2% spare pieces are included with each bulk order at no extra cost.

Test footage

Thickness readings, a salt-spray test and a pull test

These are our own thickness readings and test videos. Each reading applies to the sample that was measured, not to a whole batch.

  • Coating-thickness readings on the measuring software screen, with a gold-colored sample in a zip bag below
    Gold-colored sample, read on a coating thickness tester and its measuring software
  • Coating-thickness readings on the measuring software screen, with a gold-colored sample in a zip bag marked as a test sample
    Gold-colored test sample, thickness reading
  • Printed coating-thickness readings with the rhodium-color heart pendant that was measured
    Rhodium-color heart pendant, thickness reading
  • Printed coating-thickness readings for chain samples, with a magnified view of a measured spot
    Chain samples, thickness reading
  • Printed coating-thickness readings with the gold-colored heart pendant that was measured
    Gold-colored heart pendant, thickness reading
  • Test reports
    The lab reports and factory audit we can share, by test and date.
    See the test reports
Plated pieces in a salt-spray test chamber
A chain pulled with a push-pull force gauge for pull tests

Reorders

Reorders: four things to put in your brief

  1. The approved sample to match

    Name the approved sample or earlier order the reorder should match.

  2. The specification

    Write down the material, plating, size and finish, and ask us to check them before production starts.

  3. Changes to material or plating

    Say whether you want a new sample before any material or plating change.

  4. Inspection against the approved sample

    Pieces go through incoming (IQC) and outgoing (FQC) inspection to GB/T 2828.1. Ask if you also want them checked against the approved sample.

A staff member running a wax injector at her bench

AQL, lab and reports

Questions about quality control

Our AQL, who tests our materials, what a failed check means and how to get a full report.

Ask for a report or a test
Which AQL do you inspect to?

AQL 2.5 for major and AQL 4.0 for minor defects, in incoming (IQC) and outgoing (FQC) inspection to GB/T 2828.1.

Who tests your materials?

An outside lab. Our reports come from third-party lab tests by CTT, and each one names Lucky Forever Hardware Products Dongguan Co., Ltd. as the applicant.

What happens if a sampling check fails?

If a sampling check fails, we inspect the whole batch before it ships, and rework or scrap the defective pieces.

Can I get the full test report?

Yes, we send full reports on request. Each report covers only the samples that were tested, so your own styles need their own testing.

Next step

Ask for a report or a test

Tell us what you sell and where, and any other test you need, and we will send the reports we hold. If you want the inspection record for your order, say so in your brief.

  • Style or material

    A photo, item number or the base metal and finish.

  • Market

    The countries you sell in, and any retailer requirements.

  • Tests you need

    A test list from your retailer or compliance team, if you have one.

  • Quantity and date

    The order size and when you need the goods.

Send files by replying to our email or on WhatsApp.

One quick check, then we send your brief.

First reply within 12 hours, a quote within 24 hours.

See how we use your details in our Privacy notice.

Chat on WhatsApp